SANDING SEALER: ANOTHER VIEW
By Bruce Kunz (MCA Resin Depot South and.home eanoe builder)

I always prep with sanding sealer, but I make sure I get the right kind.
I have built five canoes in the last 22 years and know of at least 30 others.in
the same period that have not had a problem with sanding sealer. BUT—
there is more than one kind of sanding sealer! I use Durathane from Coast-
to-Coast Hardware. It says on the back of the can, "A clear polyurethane
sealer which can be used under conventional alkyd or polyurethane clear
coatings." The key here is POLYURETHANE. That's the same polyurethane
that we use over polyester and epoxy resin to finish and refinish our canoes.
Hardware Hank's also makes a compatible polyurethane-based sanding sealer
(it says so on the back of the ean). Sherwin-Williams’ sanding sealer says,
"Do not use under polyurethane." I don't. My rule of thumb is, stay with the
same chemical group, use plastic with plastic.

Why use sanding sealer at all? First, it will allow you to get rid of the
Home Builders Hallmark, glue smears you thought were sanded out, forever
preserved under glass and resin. It gives you the chance to go back and
resand those spots. Second, it will fill up the small holes left by the 9/16-
inch staples so you don't end up with starved-out pinholes all over the
outside of the hull. The 1/4-inch staple holes seem to fill alright with the
resin, but not the 9/16ths. Third, if you have any knots or pinknots in your
strips, they present a double problem. If they are of low pitch content, the
circular grain will soak up resin and cause a starved spot. If they are of high
pitch content (which they most often are), the heat generated from the resin
eure will cause the pitch to extrude from the knot. This pitch will repel
resin and prevent a bond. I wash the knots with acetone and put two extra
coats of sanding sealer over the two coats I normally use on the hull.

I have been told that a similar problem can occur with some wood
strips, but I have not had this problem. It seems to be more common with
redwood. I do not build redwood canoes any more, only cedar. Prolonged
contact with redwood and redwood dust has made me allergic. Maybe we
ean get Bob Brown to do an article on that subject, he has the same allergy.

Anyway, I concur with Betty Ketter, "Never put resin over paint," or
"paint"-type sanding sealer. Canoe building is a common sense project, but
make sure you read the back of the can. Another Betty quote worth
restating is "Put 10 canoe builders together and they'll give you 10 different
ways to do it. What's right? Whatever works best for you!" I'll stick with
sanding sealer. If nothing works right for you, try the WEST system.

Canoe Building Supplies

For Sale: MCA resin and fiberglass cloth. Polyester resin
with catalyst and wax (if required) is $13.00 per gallon. Four
ounce cloth, 50 inches wide, is $2.90 per yard; 7% ounce
cheesecloth, 60 inches wide, is $4.10 per yard. Rules for
purchase: Call ahead and schedule pickup time. Payment
by check or money order to Minnesota Canoe Association.
No cash. Bring a valid membership card.

Betty Ketter 561-2208 North Minneapolis

Bruce Kunz 454-7207 Eagan

HUT! 14

Article contents & approved summaries (0)

No article summaries are available for this view.