BUILDERS CORNER--SANDING AND MORE SANDING

Gene Jensen once told me that if one word best described canoe
building, it had to be Sanding.

It's a sure thing, no matter how neatly you strip, you're going
to spend some time sanding. You sand before you glass and again
after. You will have to sand your trim and between varnish coats.

Don't waste time with 100 or 120 grit sandpaper. You won't get a
decent job, no matter how long you work.

The surface of a freshly stripped canoe is a series of flat spots
and angles between the strips. You want to remove all these corners
and create a smooth curved surface. Some folks use a plane for this
job, others use a belt sander (the worst possible tool) and some of
us use a Surform.

A Surform and lots of elbow grease will get you the best surface.
This tool doesn't care which way the grain runs--it simply eats up
the high spots. I use it at a 30 to 45 degree angle to the strips
and go over the entire exterior.

Yes, it does make a lot of nasty gouges. No, don't worry about
them just yet. Remember, you're trying to hack down any ridges.

You know when you have Surformed enough because the entire
surface is full of those nasty gouges. I mean all over folks, don't
start sanding 'til it is.

When you start sanding, use an orbital sander with 36 grit. Yes,
I said 36 grit. This coarse paper will remove the gouges left by the
Surform and it will do it fast.

When all the marks are gone, it's time to switch to 60 grit.
This will remove the scratches left by the 36 grit. There is no
reason to go smoother than 60 prior to glassing.

After the hull is glassed on the outside, more sanding is
required. 60 or 80 grit seems to smooth up the glass job faster than
coarse paper.

Sand thoroughly between coats of resin, you will require less
coats if you do. Get the hull as smooth as you can with the 80 grit
before your last coat of resin.

My exterior finish will wait until the inside is done, sometimes
it waits until the boat is tested for a couple hundred miles.

My exteriors are a couple of coats of satin finish varnish with a
light hand sanding between coats. Some folks sand with finer and
finer paper and go for a luster, my boats are built to work well and
look reasonable, I'm a 100 grit finish man.

If anyone out there has found an easy way to prepare the inside,
please, Please step forward. Share your secret with us.

I start with a paint scraper, removing all the glue drips, then
some Surforming followed by a big disk sander (lazy way out). This
big disk will only get into the flat areas, so I use a 5" disk on my
drill with 36 grit paper to get into curves that the big sander won't
reach.

I end up in the stems with coarse paper wrapped around a 1 x 2
and lots of hand sanding. On my bubble sides and near the heel I use
an old hardened paint roller as a round sanding block.

After doing all I can with the disks, I start with my Ryobi palm
sander. This 1/6 sheet sander does the flats fine and will get into
some of the curves if I place a foam pad under the paper. Thank God
for Ryobies.

The trim will need sanding. Here is the time to get out the 120.
Sand it as smooth as you can before varnishing and between coats.

Yes, Gene, sanding is a big part of canoe building. When a cloud
of cedar sawdust starts rising in Apple Valley, the neighbors know
that Brown's boatworks is in operation.--Bob Brown